Spray Staining | 100-200 parts metal complex dyestuff-liquid 0-200 parts water-miscible solvent (Ethoxyethanol,isopropanol) 900-600 parts water |
Grain impregnation | 250 parts impregnation binder 50 parts penetrator 0-100 parts liquid brightening dye 700-600 parts water |
Base coat | Grain leather Corrected Grain leather 30 -50 parts pigment colors 50-100 parts 100-150 part polymer binder 150-250 parts 10-30 parts casein binder 20-50 parts 860-770 parts water 780-600 parts |
Pigment | Grain leather Corrected Grain 50-100 parts pigment colors 100-150 parts 100-200 parts polymers binders 150-250 parts 20-50 parts casein binders 50-100 parts -------- filling agents 20-50 parts -------- flow improvers 10 -30 parts 830 – 650 parts water 670-420 parts |
Fixation | 300 parts formaldehyde (30%) not used in common because of ban 650 parts water 0-50 parts acetic acid (6 Be⁰) |
Top coats | Casein basis 150 -300 parts casein binder 5-20 parts plasticizer 680 – 850 parts water |
Emulsion liquor 600-900 parts casein binder 100-300 parts water 0-100 parts formaldehyde 30 % | |
Nitrocellulose Lacquer or CAB lacquer 0-50 parts pigments colors 200-300 parts gloss/matt lacquer 10-20 parts plasticizers 630- 790 parts solvent | |
Polyurethane lacquer for patent leather (after application of a special base coat) 100 parts polyurethane lacquer component 120-150 parts water-free organic solvent 30-60 parts cross-linking agent | |
|
learn online leather production process,leather news and technology .All kind of leather from Pakistan leather hand gloves, leather garments and finish leather in very attractive price. To get working leather gloves made from cow split and fashion hand gloves made from sheep !Contact us irfan_gil@hotmail.com garalaboy86@gmail.com
Thursday, June 3, 2010
Genral Composition of Finishing Floats
Subscribe to:
Post Comments (Atom)
No comments:
Post a Comment